Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 6700 cP

@Shear Rate 10994 1/s,
Temperature 210 °C
6700 cP

@Shear Rate 10994 1/s,
Temperature 410 °F
ASTM D3835
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7130-1000 TPE
Product Description: StarFlex P 7130-1000 is an easy processing TPE designed for injection molding. Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades ava..