Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 10172R080 0.080" (2.3 mm) Cured Silicone Rubber Vacuum Bag

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 10172R080 0.080" (2.3 mm) Cured Silicone Rubber Vacuum Bag.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Reversion Resistant Vacuum Bag SubstrateDesign/Construction:Interleave: PolyethyleneMaterial: Cured Silicone RubberAppearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Arlon SQA-TMS-024
Thickness 63.5 microns
2.50 mil
Interleave
2030 microns
80.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
ASTM D2240
Tensile Strength 8.101 MPa
1175 psi
ASTM D412
Elongation at Break 682 %
682 %
ASTM D412
Compression Set <= 30 %
<= 30 %
Arlon SQA-TMS-017
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 72
Arlon SQA-TMS-025
Copyright © lookpolymers.com All Rights Reserved