Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SPS Guang Zhou FILLMAâ„¢ 5002F30C Mineral Filled Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer SPS Guang Zhou
Trade Name FILLMA™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SPS Guang Zhou FILLMAâ„¢ 5002F30C Mineral Filled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristic: 30%wt of Sulfate Calcium filled, low odor, good glossApplications: Household appliance parts, office suppliesInformation Provided by SPS (Guang Zhou) Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Melt Flow 15 g/10 min
15 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Flexural Strength 45.0 MPa
6530 psi
Flexural Modulus 2.50 GPa
363 ksi
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: