Material Notes:
Information provided by MetalTek
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 760 MPa
>= 110000 psi
Tensile Strength, Yield >= 690 MPa
>= 100000 psi
Elongation at Break >= 3.0 %
>= 3.0 %
Component Elements Properties Metric English Comments
Aluminum, Al 5.5 - 6.5 %
5.5 - 6.5 %
Carbon, C <= 0.20 %
<= 0.20 %
Cb + Ta 1.0 - 3.0 %
1.0 - 3.0 %
Chromium, Cr 13 - 15 %
13 - 15 %
Molybdenum, Mo 2.5 - 5.5 %
2.5 - 5.5 %
Nickel, Ni 68.55 - 77.05 %
68.55 - 77.05 %
As Balance
Titanium, Ti 0.75 - 1.25 %
0.75 - 1.25 %
Descriptive Properties Value Comments
Heat Treatment Not Heat Treated