SK Chemicals SKYPEL G163D General Grade

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP
Manufacturer SK Chemicals
Trade Name SKYPEL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SK Chemicals SKYPEL G163D General Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plastics to low hardness rubber. It is a kind of thermoplastic elastomer, which can be molded with general plastic mold by plasticizing at high temperature.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Water Absorption 0.30 %
0.30 %
24 hour; ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength, Ultimate 43.1 MPa
6260 psi
ASTM D638
Tensile Strength, Yield 10.8 MPa

@Strain 5.00 %
1560 psi

@Strain 5.00 %
ASTM D638
17.2 MPa

@Strain 10.0 %
2490 psi

@Strain 10.0 %
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Modulus 0.314 GPa
45.5 ksi
ASTM D790
Resilience 53
53
ASTM D2632
Izod Impact, Notched NB
NB
ASTM D256
Tear Strength 180 kN/m
1030 pli
ASTM D1004
Thermal Properties Metric English Comments
Melting Point 212 °C
414 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648