Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 17.2 MPa @Strain 10.0 % |
2490 psi @Strain 10.0 % |
ASTM D638 |
SK Chemicals SKYPEL G163D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |