Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 10.8 MPa @Strain 50.0 % |
1570 psi @Strain 50.0 % |
ISO 527-1/-2 |
DSM Arnitel® EB500 Polyether Ester Elastomer (European and Asian Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 10.8 MPa @Strain 5.00 % |
1560 psi @Strain 5.00 % |
ASTM D638 |
SK Chemicals SKYPEL G163D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tensile Strength, Yield | 10.8 MPa @Strain 100 % |
1560 psi @Strain 100 % |
ASTM D412 |
SK Chemicals SKYTHANE® 190A R series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 10.8 MPa @Strain 50.0 % |
1560 psi @Strain 50.0 % |
ASTM D638 |
Samyang Triel® 5401BM Thermoplastics Polyetherester Elastomer, Blow Molding Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5401BM is for blow molding applications.Applications: Automotive - CVJB and BellowsInformation provided .. |
|||
Tensile Strength, Yield | 10.8 MPa @Strain 10.0 % |
1560 psi @Strain 10.0 % |
ASTM D638 |
SK Chemicals SKYPEL G355D Special Grade Flexibility-Resistant Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tensile Strength, Yield | 10.8 MPa @Strain 100 % |
1570 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® PL420-H Injection Molding Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 10.8 MPa @Strain 100 % |
1570 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® PL420-H Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 10.8 MPa @Strain 50.0 % |
1570 psi @Strain 50.0 % |
ISO 527-1/-2 |
DSM Arnitel® EB464 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 10.8 MPa @Strain 5.00 % |
1560 psi @Strain 5.00 % |
ASTM D638 |
Samyang Triel® 5550 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5550 is an extrusion grade.Information provided by Samyang. |