Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 14.79 MPa @Temperature 136 °C, Time 605000 sec |
2145 psi @Temperature 277 °F, Time 168 hour |
Air Oven Aged |
S&E Specialty Polymers TufFlex™ GA-94-244B PVC Compound Application: 105°C rated vinyl elastomer for medical wire and cable applications. This product complies with the RoHS Directive.Information provided by S&E Specialty Polymers |