Material Notes:
Application: Flame retardant, matt finish, 90° C, flexible, oil resistant, TPE jacketing material.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.24 - 1.28 g/cc
1.24 - 1.28 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 68 - 72
68 - 72
ASTM D2240
Tensile Strength 11.7 MPa
1700 psi
ASTM D412
12.4 MPa

@Treatment Temp. 121 °C,
Time 605000 sec
1800 psi

@Treatment Temp. 250 °F,
Time 168 hour
Oven
13.45 MPa

@Treatment Temp. 100 °C,
Time 346000 sec
1951 psi

@Treatment Temp. 212 °F,
Time 96.0 hour
ATM Oil #2
Elongation at Break 400 %
400 %
ASTM D412
336 %

@Treatment Temp. 100 °C,
Time 346000 sec
336 %

@Treatment Temp. 212 °F,
Time 96.0 hour
ATM Oil #2
368 %

@Treatment Temp. 121 °C,
Time 605000 sec
368 %

@Treatment Temp. 250 °F,
Time 168 hour
Oven
Thermal Properties Metric English Comments
Brittleness Temperature -50.0 °C
-58.0 °F
ASTM D746
Oxygen Index 28 %
28 %
ASTM D2863