Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 12.4 MPa | 1800 psi | ASTM D412 |
S&E Specialty Polymers CPE-01-266A-405 Black PVC Application: 90° C, oil resistant CPE based, FT4, 210,000 BTU wire and cable jacketing material with enhanced tear properties and flexibility.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 12.4 MPa | 1800 psi | ASTM D412 |
S&E Specialty Polymers CPE-01-266LT PVC Application: 90°C, oil resistant CPE based, FT4, 210,000 BTU wire and cable jacketing material with enhanced low temperature properties.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 12.4 MPa | 1800 psi | ASTM D412 |
S&E Specialty Polymers GF-6107 PVC Description: PVC/Nitile alloy material designed for work boot applicationsInformation provided by S&E Specialty Polymers |
|||
Tensile Strength | 12.4 MPa @Treatment Temp. 121 °C, Time 605000 sec |
1800 psi @Treatment Temp. 250 °F, Time 168 hour |
Oven |
S&E Specialty Polymers GTPE-2272ALC PVC Application: Flame retardant, matt finish, 90° C, flexible, oil resistant, TPE jacketing material.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | >= 12.4 MPa | >= 1800 psi | ASTM D638 |
S&E Specialty Polymers GTPO 9100HF Series PVC Application: New generation 80/90C, UV Resistant, low gravity, flexible, polyolefin based Zero Halogen compound with good physical characteristics.Information provided by S&E Specialty Pol.. |
|||
Tensile Strength | >= 12.4 MPa | >= 1800 psi | ASTM D638 |
S&E Specialty Polymers GTPO8102BA-H NATURAL PVC Application: High-flow flame retardant TPO compound for insulation and jacketing compound designed for ribbon cable applications. The flame retardant package incorporates non-PDBPO, PBB, PBDE flame-.. |
|||
Tensile Strength | 12.4 MPa | 1800 psi | ASTM D412 |
S&E Specialty Polymers GTPO8290FR-75 RoHS PVC Application: RoHS compliant, flexible flame retardant thermoplastic olefin compound.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 12.4 MPa | 1800 psi | ASTM D412 |
S&E Specialty Polymers TufFlex™ GA-1042FR-60-0-405 Black TPE Compound Application: An oil resistant, flexible, 60°C rated jacketing compound.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 12.4 MPa | 1800 psi | ASTM D412 |
S&E Specialty Polymers TufFlex™ GF 6107 PVC/Nitrile Alloy Application: PVC/Nitrile alloy material designed for work boot midsole applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 12.4 MPa | 1800 psi | ASTM D412 |
S&E Specialty Polymers TufFlex™ GTPE-2272 TPE Compound Application: A 105°C flexible, oil resistant, flame retardant TPE jacketing material designed for SJEO applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | >= 12.4 MPa | >= 1800 psi | ASTM D412 |
S&E Specialty Polymers TufGuard E™ GTPO8102BA-H-Natural TPO, Flame Retardant Application: High-flow flame retardant TPO compound for insulation and jacketing designed for ribbon cable applications. The flame retardant package incorporates non-PDBPO, PBB, PBDE flame retardant.. |
|||
Tensile Strength | 12.4 MPa | 1800 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-3174 PVC Compound Application: 80°C PVC General Purpose Jacketing compound with high gloss surface.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 12.4 MPa | 1800 psi | ASTM D412 |
Northstar Polymers MPP-A90A High Performance Polyether This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex.. |
|||
Tensile Strength | 12.4 MPa @Strain 100 % |
1800 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV 3432 Trans 9000 Polyvinyl Chloride, Flexible (PVC, Flexible) This product has received full compliance certification for USP Biological Reactivity Tests under USP Plastic Class VI.NOTE: All ingredients used in the formulation of this compound are listed in th.. |
|||
Tensile Strength | 12.4 MPa @Strain 100 % |
1800 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3432 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength | 12.4 MPa @Strain 100 % |
1800 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3860 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength | 12.4 MPa @Strain 100 % |
1800 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3887 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength | 12.4 MPa @Strain 100 % |
1800 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B5DG1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 12.4 MPa | 1800 psi | Typical |
Garlock 7797 Neoprene Sheet Rubber This blended neoprene sheet is used where good oil, petroleum, ozone and weathering-resistance is needed.Black, smooth cloth finishInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | 12.4 MPa | 1800 psi | across grain; ASTM F152 |
Garlock 9850 Compressed Carbon Fiber Gasketing, Nitrile Binder Carbon fibers with a nitrile binder.Carbon fiber gasketing excels in harshest conditions - intense heat, high pressure, saturated steam and hot oils.Laboratory-tested for fire safety.Long-lasting se.. |
|||
Tensile Strength | 12.4 MPa | 1800 psi | across grain; ASTM F152 |
Garlock 9900 Compressed Graphite Fiber Gasketing, Nitrile Binder Graphite fibers with a nitrile binder.Graphite fiber gasketing withstands extreme temperatures and pressures, as well as many chemicalsPassed Garlock Fire tests, and is ABS Fire Safe Type ApprovedLo.. |
|||
Tensile Strength | 12.4 MPa | 1800 psi | across grain; ASTM F152 |
Garlock GYLON® 3565 ENVELON® PTFE Gasketing, Glass Microsphere Filled PTFE with aluminosilicate microsphere filler.Soft, deformable exterior conforms to surface irregularities; ideal for worn, warped or pitted flangesStable blue core improves cold flow resistanceLow b.. |
|||
Tensile Strength | 12.4 MPa | 1800 psi | Typical |
Garlock SBR Extruded Skirtboard SBR rubber extruded skirtboard for protection applicationsInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | 12.4 MPa | 1800 psi | ASTM D638 |
Saint-Gobain Rulon® W2 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Tensile Strength | 12.4 MPa | 1800 psi | ASTM D412 |
Saint-Gobain Tygon® S3™ E-LFL Long-Flex Life Pump Tubing Formulation Tygon S3™ E-LFL from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-base.. |
|||
Tensile Strength | 12.4 MPa | 1800 psi | |
Teknor Apex Telcar® TL-3050-88 Thermoplastic Elastomer Temperature Ratings: Wet Location: 75°C, Dry Location: 90°C Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength | 12.4 MPa | 1800 psi | ASTM D638 |
Ensinger Tecatron® XP-73 Compression Molded PPS Compound, 60% PTFE Seal Material Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Strength | 12.4 MPa | 1800 psi | |
AlphaGary Garathane™ X 94-350 B Polyurethane based compound Flame retardant polyether based polyurethane |
|||
Tensile Strength | 12.4 MPa | 1800 psi | |
Teknor Apex Elexar® EL 8730R Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical properti.. |
|||
Tensile Strength | 12.4 MPa @Strain 100 % |
1800 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3905 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |