Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 11.7 MPa | 1700 psi | ASTM D412 |
S&E Specialty Polymers GFE-1815 PVC Description: Expandable PVC/Nitrile, oil resistantInformation provided by S&E Specialty Polymers |
|||
Tensile Strength | 11.7 MPa | 1700 psi | ASTM D412 |
S&E Specialty Polymers GTPE-2272ALC PVC Application: Flame retardant, matt finish, 90° C, flexible, oil resistant, TPE jacketing material.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 11.7 MPa | 1700 psi | ASTM D412 |
S&E Specialty Polymers TufFlex™ GF 1815 PVC/Nitrile Alloy Application: A flexible, PVC/Nitrile, oil resistant compound suitable for footwear applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 11.7 MPa | 1700 psi | ASTM D638 |
Quadrant EPP Proteus® LDPE - Low Density Polyethylene (ASTM Product Data Sheet) |
|||
Tensile Strength | 11.7 MPa @Strain 100 % |
1700 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2185 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2185 is a 85 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2185 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Tensile Strength | 11.7 MPa @Strain 100 % |
1700 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2185G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2185G is a 85 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2185G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Tensile Strength | 11.7 MPa @Strain 100 % |
1700 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 11.7 MPa @Strain 100 % |
1700 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B5D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 11.7 MPa @Strain 100 % |
1700 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B5D02 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 11.7 MPa | 1700 psi | Typical |
Garlock 362 Nitrile Sheet Rubber Nitrile sheet is primarily used for applications where resistance to oil, solvents and fuels is required.Style #362 is a white nitrile sheet made from FDA-approved ingredients per Z1 CFR 177.2600. I.. |
|||
Tensile Strength | 11.7 MPa | 1700 psi | Typical |
Garlock 563 EPDM Sheet Rubber Excellent general purpose gasket materials for air, hot and cold water, saturated steam and exterior service.Black, smooth finish. Excellent resistance to weathering, ozone and UV exposure. It prov.. |
|||
Tensile Strength | 11.7 MPa | 1700 psi | ASTM D638 |
Saint-Gobain Rulon® XL Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Tensile Strength | 11.7 MPa | 1700 psi | |
Teknor Apex Elexar® EL 8732R Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Tensile Strength | 11.7 MPa | 1700 psi | |
AlphaGary AG 005 4B Styrenic Thermoplastic Elastomer Styrenic based TPE molding grade compound. Application example includes airbag cover |
|||
Tensile Strength | 11.7 MPa | 1700 psi | |
AlphaGary Megolon™ HF 8142 UV Low Smoke Halogen Free 105°C Rated HFFR Jacket and Buffer Compound. UV resistant. Application examples include Data Cables, Optical Cables. |
|||
Tensile Strength | 11.7 MPa | 1700 psi | |
AlphaGary Megolon™ HF 8037 DD Low Smoke Halogen Free MEGOLON™ HF 8037 DD is a low die drool, flame retarded, zero halogen jacketing compound |
|||
Tensile Strength | 11.7 MPa | 1700 psi | |
AlphaGary Megolon™ HF 8142 Low Smoke Halogen Free 105°C Rated HFFR Jacket and Buffer Compound. Application examples include Data Cables, Optical Cables. |
|||
Tensile Strength | 11.7 MPa | 1700 psi | |
AlphaGary AlphaSeal™ 240-6CY Blue 7002 Polyolefin Thermoplastic Elastomer AlphaSeal™ 240-6CY Blue 7002 is recommended for liners for plastic caps for carbonated soft drinks. It is formulated for low taste and odor and exhibits good elastic recovery, abrasion resistance a.. |