Mechanical Properties Metric English Comments
Tensile Strength 13.45 MPa

@Treatment Temp. 100 °C,
Time 346000 sec
1951 psi

@Treatment Temp. 212 °F,
Time 96.0 hour
ATM Oil #2
S&E Specialty Polymers GTPE-2272ALC PVC
Application: Flame retardant, matt finish, 90° C, flexible, oil resistant, TPE jacketing material.Information provided by S&E Specialty Polymers