Mechanical Properties Metric English Comments
Tensile Strength 11.7 MPa
1700 psi
ASTM D412
S&E Specialty Polymers GFE-1815 PVC
Description: Expandable PVC/Nitrile, oil resistantInformation provided by S&E Specialty Polymers
Tensile Strength 11.7 MPa
1700 psi
ASTM D412
S&E Specialty Polymers GTPE-2272ALC PVC
Application: Flame retardant, matt finish, 90° C, flexible, oil resistant, TPE jacketing material.Information provided by S&E Specialty Polymers
Tensile Strength 11.7 MPa
1700 psi
ASTM D412
S&E Specialty Polymers TufFlex™ GF 1815 PVC/Nitrile Alloy
Application: A flexible, PVC/Nitrile, oil resistant compound suitable for footwear applications.Information provided by S&E Specialty Polymers
Tensile Strength 11.7 MPa
1700 psi
ASTM D638
Quadrant EPP Proteus® LDPE - Low Density Polyethylene (ASTM Product Data Sheet)
Tensile Strength 11.7 MPa

@Strain 100 %
1700 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ HC 2185 Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon HC 2185 is a 85 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2185 can be used for extrusion and injection molding healthcare applications.NOTE: All ing..
Tensile Strength 11.7 MPa

@Strain 100 %
1700 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ HC 2185G Polyvinyl Chloride, Flexible (PVC, Flexible)
Geon HC 2185G is a 85 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2185G can be used for extrusion and injection molding healthcare applicatio..
Tensile Strength 11.7 MPa

@Strain 100 %
1700 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible B5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 11.7 MPa

@Strain 100 %
1700 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible B5D00 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 11.7 MPa

@Strain 100 %
1700 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible B5D02 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 11.7 MPa
1700 psi
Typical
Garlock 362 Nitrile Sheet Rubber
Nitrile sheet is primarily used for applications where resistance to oil, solvents and fuels is required.Style #362 is a white nitrile sheet made from FDA-approved ingredients per Z1 CFR 177.2600. I..
Tensile Strength 11.7 MPa
1700 psi
Typical
Garlock 563 EPDM Sheet Rubber
Excellent general purpose gasket materials for air, hot and cold water, saturated steam and exterior service.Black, smooth finish. Excellent resistance to weathering, ozone and UV exposure. It prov..
Tensile Strength 11.7 MPa
1700 psi
ASTM D638
Saint-Gobain Rulon® XL Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Tensile Strength 11.7 MPa
1700 psi
Teknor Apex Elexar® EL 8732R Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
Tensile Strength 11.7 MPa
1700 psi
AlphaGary AG 005 4B Styrenic Thermoplastic Elastomer
Styrenic based TPE molding grade compound. Application example includes airbag cover
Tensile Strength 11.7 MPa
1700 psi
AlphaGary Megolon™ HF 8142 UV Low Smoke Halogen Free
105°C Rated HFFR Jacket and Buffer Compound. UV resistant. Application examples include Data Cables, Optical Cables.
Tensile Strength 11.7 MPa
1700 psi
AlphaGary Megolon™ HF 8037 DD Low Smoke Halogen Free
MEGOLON™ HF 8037 DD is a low die drool, flame retarded, zero halogen jacketing compound
Tensile Strength 11.7 MPa
1700 psi
AlphaGary Megolon™ HF 8142 Low Smoke Halogen Free
105°C Rated HFFR Jacket and Buffer Compound. Application examples include Data Cables, Optical Cables.
Tensile Strength 11.7 MPa
1700 psi
AlphaGary AlphaSeal™ 240-6CY Blue 7002 Polyolefin Thermoplastic Elastomer
AlphaSeal™ 240-6CY Blue 7002 is recommended for liners for plastic caps for carbonated soft drinks. It is formulated for low taste and odor and exhibits good elastic recovery, abrasion resistance a..