Material Notes:
Product Description: PP 528K is formulated with an advanced nucleating additive and was specially developed for in-line and off-line thermoforming applications. PP528K exhibits the following features.High stiffnessGood clarityVery good dimensional stabilityEasy processability and faster cyclingTypical Applications: PP 528K is used for the production of various containers, mainly for food and health drink products such as cups, trays and lids.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102
102
ASTM D785
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus, 1% Secant 1850 MPa
268000 psi
ASTM D790A
Izod Impact, Notched 0.350 J/cm
0.656 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525B