SABIC Innovative Plastics ULTEM 2410 PEI (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name ULTEM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics ULTEM 2410 PEI (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
ISO 1183
Moisture Absorption 0.400 %
0.400 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.80 %
0.80 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
on Tensile Bar; SABIC Method
Melt Index of Compound 7.0 g/10 min

@Load 5.00 kg,
Temperature 360 °C
7.0 g/10 min

@Load 11.0 lb,
Temperature 680 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 170 MPa
24700 psi
ISO 2039-1
Tensile Strength at Break 180 MPa
26100 psi
5 mm/min; ISO 527
Elongation at Break 2.0 %
2.0 %
5 mm/min; ISO 527
Tensile Modulus 11.5 GPa
1670 ksi
1 mm/min; ISO 527
Flexural Strength 240 MPa
34800 psi
2 mm/min; ISO 178
Flexural Modulus 10.0 GPa
1450 ksi
2 mm/min; ISO 178
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*4; ISO 180/1U
35.0 kJ/m²

@Temperature -30.0 °C
16.7 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Taber Abrasion, mg/1000 Cycles 20
20
CS-17, 1 kg; SABIC Method
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 23.0 - 150 °C
8.33 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
CTE, linear, Transverse to Flow 45.0 µm/m-°C

@Temperature 23.0 - 150 °C
25.0 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
Thermal Conductivity 0.290 W/m-K
2.01 BTU-in/hr-ft²-°F
ISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 217 °C
423 °F
Rate B/50; ISO 306
225 °C
437 °F
Rate B/120; ISO 306
230 °C
446 °F
Rate A/50; ISO 306
Glass Transition Temp, Tg 217 °C
423 °F
UL RTI, Electrical 105 °C
221 °F
UL 746B
UL RTI, Mechanical with Impact 105 °C
221 °F
UL 746B
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
Flammability, UL94 V-0

@Thickness 0.250 mm
V-0

@Thickness 0.00984 in
UL 94
5VA

@Thickness 1.50 mm
5VA

@Thickness 0.0591 in
UL 94
Oxygen Index 48 %
48 %
ISO 4589
Glow Wire Test 960 °C

@Thickness 3.20 mm
1760 °F

@Thickness 0.126 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ROA; IEC 60093
Dielectric Constant 3.1

@Frequency 1.00e+6 Hz
3.1

@Frequency 1.00e+6 Hz
IEC 60250
3.5

@Frequency 50.0 - 60.0 Hz
3.5

@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 16.0 kV/mm

@Thickness 3.20 mm
406 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
26.0 kV/mm

@Thickness 1.60 mm
660 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
35.0 kV/mm

@Thickness 0.800 mm
889 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
Dissipation Factor 0.0019

@Frequency 1.00e+6 Hz
0.0019

@Frequency 1.00e+6 Hz
IEC 60250
0.0025

@Frequency 50.0 - 60.0 Hz
0.0025

@Frequency 50.0 - 60.0 Hz
IEC 60250
Comparative Tracking Index >= 100 V
>= 100 V
IEC 60112
150 V
150 V
IEC 60112
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2