Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 170 MPa | 24700 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Hardness, H358/30 | 170 MPa | 24700 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 2400F PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be.. |
|||
Hardness, H358/30 | 170 MPa | 24700 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Hardness, H358/30 | 170 MPa | 24700 psi | ISO 2039-1 |
SABIC Innovative Plastics Ultem 2410F PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). UL94 V0 and 5VA listing. US FDA and European Food contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Hardness, H358/30 | 170 MPa | 24700 psi | ISO 2039-1 |
SABIC Innovative Plastics ULTEM 2410R PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Hardness, H358/30 | 170 MPa | 24700 psi | ISO 2039-1 |
SABIC Innovative Plastics Ultem PW2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water
applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and.. |
|||
Hardness, H358/30 | 170 MPa | 24700 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East) Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors |