Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746 |
PolyOne Maxxam™ FR PP 401 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746 |
PolyOne Maxxam™ PP CS 75 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
UL RTI, Mechanical without Impact | 105 °C @Temperature 105 °C |
221 °F @Temperature 221 °F |
UL 746 |
PolyOne Novablend™ 6602 Polyvinyl Chloride, Rigid (PVC, Rigid) Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: .. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Asia Pacific) PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Asia Pacific) PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1200HF is the improved version of CYCOLOY C1200 and has been developed to provide enhanced productivity and surface appearance for |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810SK is a multi purpose PC+ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLOY FXC810SK is suitable for those applications that require sparkl.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL746B |
Idemitsu Kosan Xarec® WA 210 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified, Improved Mold Release. Used in Automotive and Industrial applications. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | |
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, Dry as Molded Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM 2110EPR PEI (Asia Pacific) 10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM 2210EPR PEI 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Ultem 2313 PEI (Asia Pacific) 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific regi.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM 2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM 4000 PEI Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM 4000 PEI (Asia Pacific) Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5111 PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5201 PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Ultem CRS5211 PEI 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Th.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Ultem CRS5211 PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Thi.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5311 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM UC1200 PEI (Asia Pacific) 12% carbon fiber reinforced Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 listing in recognized colors. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Valox® 745 PBT 30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Valox® 365 PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031".This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746 |
Styron EMERGEâ„¢ 4410-18 MFR Polycarbonate EMERGEâ„¢ PC 4410-18 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL 731S PPE+PS (Asia Pacific) High heat PPO/HIPS alloy suitable for use in some potable water applications. |
|||
UL RTI, Mechanical without Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer |