Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Noryl PX6592 PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Noryl PX6592 PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% glass filled, PPO/HIPS alloy.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 88.0 MPa
12800 psi
Type I, 50 mm/min; ASTM D 638
Elongation at Break 5.0 %
5.0 %
Type I, 50 mm/min; ASTM D 638
Flexural Yield Strength 125 MPa
18100 psi
1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 5.20 GPa
754 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 0.580 J/cm

@Temperature 23.0 °C
1.09 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 120 °C

@Thickness 3.20 mm
248 °F

@Thickness 0.126 in
unannealed; ASTM D 648
132 °C

@Thickness 6.40 mm
270 °F

@Thickness 0.252 in
unannealed; ASTM D 648
Users viewing this material also viewed the following: