Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 120 °C @Thickness 3.20 mm |
248 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl PX6592 PPE+PS (Asia Pacific) 20% glass filled, PPO/HIPS alloy.This data was supplied by SABIC-IP for the Asia Pacific region. |