Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.20 GPa | 754 ksi | |
Plastcom SLOVAMID 6 GF 5 T 20 FRG 2 PA6, 5% glass fibre, 20% mineral filling FeaturesPA 6 for injection moulding, with halogen free flame retardant based on polyphosphate. Good anisotrophi shinking. Application for the electrical industry: protectors, coil forms, covers, ter.. |
|||
Flexural Modulus | 5.20 GPa @Temperature 23.0 °C |
754 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYabs T00 GF20 ABS, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 5.20 GPa @Temperature 23.0 °C |
754 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT D234 GF30 FR PBT, Glass-Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXE4472L PC (Asia Pacific) Lexan* FXE4472L is a 20% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | |
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre, 20% glass beads FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre and 20% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PX6592 PPE+PS (Asia Pacific) 20% glass filled, PPO/HIPS alloy.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East) VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Unitika M1030E PA6, Dry Nano composite nylonInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 5.20 GPa @Temperature 160 °C |
754 ksi @Temperature 320 °F |
ISO 178 |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GS 50 HWCP 50% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | dry; ISO 178 |
DSM Akulon® K224-G3-FC NA99001 PA6-GF15 15% Glass Reinforced |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Ashley Polymers Ashlene® 527-25G Nylon 66, 25% Glass Reinforced A 25% glass reinforced impact modified Nylon 66.Data provided by the manufacturer |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Ashley Polymers Ashlene® ABS Resin R2018, 18% Glass Reinforced General purpose, 18% glass reinforced ABS resin.Data provided by the manufacturer |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Chem Polymer Chemlon 115 G Nylon 66, 15% Glass Fiber Reinforced A 15% glass fiber reinforced nylon 66 offering improved creep resistance, stiffness, tensile strength and dimensional stability over unmodified nylon 66 materials. This product offers slight improv.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Adell BT-14 Nylon 6, 20% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Ashley Polymers Ashlene® 830L-13G Nylon 6, 13% Glass Reinforced A 13% glass fiber reinforced Nylon 6 designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 type materials.Data p.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 621 Nylon 6/6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Ashley Polymers Ashlene® R3145-20G PC/PBT Alloy, 20% Glass Reinforced A 20% glass reinforced alloy for high impact, increased mechanical strength, chemical resistance, and thermal properties.Data provided by the manufacturer |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
Polyram Polytron P30N07 Polypropylene, 30% Long Glass Fiber, UV Stabilized A chemically coupled 30% LGF reinforced natural PP, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Owens Corning Glass Fiber Reinforced Polyphenylene Oxide (PPO), 20 wt.% glass Polyphenylene Oxide provides excellent resistance to aqueous media. It is softened by aromatic hydrocarbons. Data provided by the manufacturer, Owens Corning. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | Tangent, 0.05 in/min; ASTM D790 |
LyondellBasell Hostacom™ PF062-3 Polypropylene Homopolymer Description: Hostacom™ PF062-3 high melt flow, 5,200 MPa flexural modulus, chemically coupled, 30% glass fiber-reinforced polypropylene homopolymer has good impact strength, high stiffness and very.. |