Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.20 GPa | 754 ksi | STN EN ISO 178 |
Plastcom SLOVAMID 6 GF 15 Polyamide 6, 15% Glass Fiber FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and .. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Nylene® PA6 Glass Filled 5213 HS Nylon 6 13% Glass Filled; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Modulus | 5.20 GPa @Temperature 23.0 °C |
754 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT D234 GF30 FR PBT, Glass-Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | |
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre, 20% glass beads FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre and 20% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri.. |
|||
Flexural Modulus | 5.20 GPa @Temperature 23.0 °C |
754 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT C213 GF15 FR PBT, Glass Fiber-Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Modulus | 5.20 GPa @Temperature 23.0 °C |
754 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT D211 GF10 PBT, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
North Wood Plastics PS with 40% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DX00714H PC LNP LUBRICOMP* DX00714H is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Wear Resistant, Healthcare. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, Conditioned Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Appl.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East) VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East) VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 2F005 ETFE LNP* Thermocomp* 2F005 is a fluoropolymer compound based on ETFE containing 25% Glass Fiber. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Unitika M1030E PA6, Dry Nano composite nylonInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 5.20 GPa @Temperature 160 °C |
754 ksi @Temperature 320 °F |
ISO 178 |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GS 50 HWUVCP 50% Glass Sphere Filled Nylon 6, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000/52 GV 15 HWCP 15% Glass Fiber Nylon 6, Low Temperature Impact Modified, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | dry; ISO 178 |
DSM Akulon® K224-G3-FC NA99001 PA6-GF15 15% Glass Reinforced |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Adell BH-18 Nylon 6, 40% Mineral Filled Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM Test |
BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Dry) Ultramid 8231G HS BK-102 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Adell BT-14 Nylon 6, 20% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Adell EQ-18 Homopolymer Polypropylene, 40% Mica Filled Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 621 Nylon 6/6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Owens Corning Glass Fiber Reinforced Polyphenylene Oxide (PPO), 20 wt.% glass Polyphenylene Oxide provides excellent resistance to aqueous media. It is softened by aromatic hydrocarbons. Data provided by the manufacturer, Owens Corning. |