SABIC Innovative Plastics NORYL HM4025H PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL HM4025H PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% GF/MF filled FR PPE/PS blend, high flow
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0015 - 0.0025 cm/cm

@Thickness 3.20 mm
0.0015 - 0.0025 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 15.4 g/10 min

@Load 2.16 kg,
Temperature 300 °C
15.4 g/10 min

@Load 4.76 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 90
90
ASTM D785
Tensile Strength, Yield 116 MPa
16800 psi
SABIC - Japan Method
Elongation at Break 4.0 - 6.0 %
4.0 - 6.0 %
SABIC - Japan Method
Flexural Strength 154 MPa
22300 psi
ASTM D790
Flexural Modulus 10.29 GPa
1492 ksi
ASTM D790
Izod Impact, Notched 0.680 J/cm
1.27 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 21.0 - 33.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.7 - 18.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 125 °C

@Thickness 6.40 mm
257 °F

@Thickness 0.252 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Users viewing this material also viewed the following: