SABIC Innovative Plastics NORYL EZ250 PPE+PS

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL EZ250 PPE+PS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Automotive wheel covers. Offers superior processability/flow and better chemical resistance when exposed to many automotive fluids over PX0844.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.0 MPa
6380 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 40 %
40 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 68.0 MPa
9860 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 1.99 GPa
289 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 2.93 J/cm
5.49 ft-lb/in
ASTM D256
1.33 J/cm

@Temperature -40.0 °C
2.49 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Dart Drop, Total Energy 39.0 J
28.8 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
33.0 J

@Temperature -40.0 °C
24.3 ft-lb

@Temperature -40.0 °F
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 126 °C

@Thickness 6.40 mm
259 °F

@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 112 °C

@Thickness 6.40 mm
234 °F

@Thickness 0.252 in
unannealed; ASTM D648
Users viewing this material also viewed the following: