Polymer Property : Izod Impact, Notched = 5.49 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.93 J/cm
5.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycolac® MGABS02 ABS
General purpose ABS. Excellent flow/impact.
Izod Impact, Notched 2.93 J/cm
5.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycolac® BDT5510 ABS
Automotive. High heat resistance, low gloss, color concentratable for interior applications. Natural only.
Izod Impact, Notched 2.93 J/cm
5.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL SPN420 PPE+PS
Superior Productivity plus heat and impact resistance. Excellent processability.
Izod Impact, Notched 2.93 J/cm
5.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL SPN420 PPE+PS (Asia Pacific)
Superior Productivity plus heat and impact resistance. Excellent processability.
Izod Impact, Notched 2.93 J/cm
5.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
Izod Impact, Notched 2.93 J/cm
5.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Asia Pacific)
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
Izod Impact, Notched 2.93 J/cm
5.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Europe-Africa-Middle East)
>PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent).
Izod Impact, Notched 2.93 J/cm
5.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL N190X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications.
Izod Impact, Notched 2.93 J/cm
5.49 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL EZ250 PPE+PS
Automotive wheel covers. Offers superior processability/flow and better chemical resistance when exposed to many automotive fluids over PX0844.