Material Notes:
LNP* Thermocomp* OF003A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 77.0 MPa
11200 psi
ASTM D 638
Tensile Strength, Yield 77.0 MPa
11200 psi
ASTM D 638
Elongation at Break 1.1 %
1.1 %
ASTM D 638
Elongation at Yield 1.1 %
1.1 %
ASTM D 638
Flexural Modulus 7.03 GPa
1020 ksi
ASTM D 790
Izod Impact, Notched 0.480 J/cm

@Temperature 23.0 °C
0.899 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 0.630 J/cm

@Temperature 23.0 °C
1.18 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 194 °C

@Thickness 3.20 mm
381 °F

@Thickness 0.126 in
unannealed; ASTM D 648