SABIC Innovative Plastics LNP THERMOTUF VF003 PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOTUF VF003 PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOTUF* VF003 is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: High Impact.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 77.0 MPa
11200 psi
ASTM D638
Elongation at Break 2.6 %
2.6 %
ASTM D638
Tensile Modulus 5.01 GPa
727 ksi
50 mm/min; ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 4.48 GPa
650 ksi
ASTM D790
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.08 J/cm
11.4 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 241 °C

@Thickness 3.20 mm
466 °F

@Thickness 0.126 in
unannealed; ASTM D648