Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.08 J/cm | 11.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP LC006 PEEK LNP THERMOCOMP* LC006 is a compound based on Polyetheretherketone resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 6.08 J/cm | 11.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT LNP* STAT-LOY* WF306C is a compound based on PBT resin containing 30% Glass Fiber. Added features of this material include: Antistat, Clean Compound System. |
|||
Izod Impact, Unnotched | 6.08 J/cm | 11.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT (Asia Pacific) LNP* Stat-loy* WF306C is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: Antistat, Clean Compounding System. |
|||
Izod Impact, Unnotched | 6.08 J/cm | 11.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOTUF VF003 PA 66 LNP* THERMOTUF* VF003 is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Unnotched | 6.08 J/cm | 11.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOTUF VF003 PA 66 (Asia Pacific) LNP* THERMOTUF* VF003 is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: High Impact. |