Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOTUF PF00AIS PA 6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOTUF PF00AIS PA 6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOTUF* PF00AIS is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Physical Properties Metric English Comments
Density 1.63 g/cc
0.0589 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
ASTM D638
Flexural Strength 248 MPa
36000 psi
ASTM D790
Flexural Modulus 12.27 GPa
1780 ksi
ASTM D790
Izod Impact, Notched 1.65 J/cm
3.09 ft-lb/in
ASTM D256
Izod Impact, Unnotched 12.97 J/cm
24.30 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 204 °C

@Thickness 3.20 mm
399 °F

@Thickness 0.126 in
unannealed; ASTM D648