Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* RFB66 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass.
Physical Properties Metric English Comments
Density 1.71 g/cc
0.0618 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 151 MPa
21900 psi
ASTM D638
Elongation at Break 1.7 %
1.7 %
ASTM D638
Tensile Modulus 16.54 GPa
2399 ksi
50 mm/min; ASTM D638
Flexural Strength 248 MPa
36000 psi
ASTM D790
Flexural Modulus 13.78 GPa
1999 ksi
ASTM D790
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.67 J/cm
12.5 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 250 °C

@Thickness 3.20 mm
482 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: