Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.71 g/cc | 0.0618 lb/in³ | |
Plastcom SLOVAMID 6 GF 65 PA6, 65% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | |
Plastcom SLOVAMID 6 GF 65/1M PA6 reinforced with 65% glass fibre Features: PA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded
  AMODEL AF-1133 V0 resin in a 33% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high deflection temperature, tensile strength, and flexural modulus. The material has good d.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Plenco 501 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 501 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in heat resistant and electrical applications. It is designed for elevated temperature exposure for e.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP UFL269SA PPA (Asia Pacific) LNP* Lubricomp* UFL269SA is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Heat Stabilized,.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KB008 Acetal Copolymer LNP THERMOCOMP* KB008 is a compound based on Acetal Copolymer resin containing 40% Glass Bead. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069S PA 66 LNP THERMOCOMP* RF0069S is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Lubrizol Isoplast® 101LGF60NAT Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183-87 |
Wellman Wellamid® GF60-66/6 XE-NBK1 60% Glass Fiber Reinforced, Engineering Grade Nylon 66/6 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | DIN 53479 |
Polyram RamSter PF300J50 PBT, 50% Glass Fiber + Glass beads 50% Glass-fiber and glass beads reinforced PBT.Information provided by Polyram Ram On Ind. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK609 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**) 50% Glass Reinforced Polybutylene Terephthalate Crastin SK609 BK851 is a 50% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Ensinger Tecapeek® XP-110 Compression Molded PEEK Compound, 45% Mineral Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-61 Compression Molded PPS Compound, 25% Fiberglass and Mineral Filled Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
Eurotec® Tecopet® PT70 GR30 NL100 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.71 g/cc @Temperature 23.0 °C |
0.0618 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Dry, 60% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | Liquid |
3M Fluorinert™ FC-3284 Electronic Liquid 3M™ Fluorinert™ Liquid FC-3284 is a non-conductive, thermally and chemically stable fluid ideal for use in single and two phase heat transfer fluid applications, such as semiconductor package test.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO R 1183 |
Multibase Multibatch® MP 52255 Injection Molding HPP. 70% CaCO3 Filled.Information provided by Multibase |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
Polyplastic Armlen® PE MF 70-2FR Magnesium Hydroxide Filled Polyethylene 70% Magnesium HydroxideFor extrusion of fire resistant aluminum composite panels.Information provided by PolyPlastic Group. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | Dry As Molded |
Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, at 50% RH
(di AMODEL AF-1133 V0 resin in a 33% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high deflection temperature, tensile strength, and flexural modulus. The material has good d.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RV00CES PA 66 LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RV00CES PA 66 LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 (Asia Pacific) LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 (Asia Pacific) LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | |
LATI Laticonther 80 GR/50 PPS, 50% Graphite Reinforced High thermal conductivity product based on Polyphenylene Sulfide (PPS). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |