SABIC Innovative Plastics LNP THERMOCOMP RC008ESS PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP RC008ESS PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* RC008ESS is a compound based on PA66 resin containing Carbon Fiber. Added features include; Electrically Conductive, Easy Molding, Heat Stabilized.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0080 cm/cm

@Time 86400 sec
0.0080 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength, Yield 254 MPa
36800 psi
5 mm/min; ISO 527
Elongation at Break 2.7 %
2.7 %
5 mm/min; ISO 527
Tensile Modulus 22.9 GPa
3320 ksi
1 mm/min; ISO 527
Flexural Yield Strength 375 MPa
54400 psi
2 mm/min; ISO 178
Flexural Modulus 24.6 GPa
3570 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 70.0 kJ/m²
33.3 ft-lb/in²
80*10*4; ISO 180/1U
Electrical Properties Metric English Comments
Surface Resistance 10 - 100 ohm
10 - 100 ohm
ASTM D257