Indium Corp. Indalloy® 84001 Flux #1 Paste Flux containing Ammonium Chloride

Category Ceramic , Halide
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 84001 Flux #1 Paste Flux containing Ammonium Chloride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Indalloy Flux #1 is a non-acid, non toxic, Pb-free, amber colored paste flux for use on copper, brass, galvanized iron, lead, zinc, tin, silver, nickel, mild steel, terne plate and malleable iron. Its strong detergent action cleans as it solders.Chloride Content: Contains Ammonium Chloride (No Zinc Chloride)Due to its possible corrosive nature, Indalloy Flux #1 is not recommended for electronics applications.Cleaning: Warm water (< 50°C) and mechanical scrubbingSolder Alloy Compatibility: Indalloy Flux #1 works well with all common soft solders. The chlorine content may cause corrosion of indium based solders.Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
pH 6.5 - 7.0
6.5 - 7.0
Thermal Properties Metric English Comments
Active Range 100 - 338 °C
212 - 640 °F
Flash Point >= 204 °C
>= 399 °F