Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wieland Simidur Superior PFM Alloy

Category Metal , Nonferrous Metal , Precious Metal , Palladium Alloy
Manufacturer Wieland
Trade Name Simidur
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland Simidur Superior PFM Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partialsDental
Physical Properties Metric English Comments
Density 11.7 g/cc
0.423 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 200
200
HV5/30; after porcelain firing
230
230
HV5/30; hardened
Tensile Strength, Yield 378.9 MPa

@Strain 0.200 %
54960 psi

@Strain 0.200 %
after porcelain firing
519.5 MPa

@Strain 0.200 %
75350 psi

@Strain 0.200 %
hardened
Elongation at Break 17 %
17 %
hardened
34 %
34 %
after porcelain firing
Modulus of Elasticity 113 GPa
16400 ksi
Thermal Properties Metric English Comments
CTE, linear 14.5 µm/m-°C

@Temperature 25.0 - 500 °C
8.06 µin/in-°F

@Temperature 77.0 - 932 °F
Component Elements Properties Metric English Comments
Gold, Au 63.5 %
63.5 %
Silver, Ag 23.4 %
23.4 %
Processing Properties Metric English Comments
Processing Temperature 849 °C
1560 °F
Preheating Temp.
Melt Temperature 1210 - 1290 °C
2210 - 2350 °F
Casting Temperature 1400 °C
2550 °F
Descriptive Properties Value Comments
Color white