Description: Clarified, Excellent Mold Release, Excellent Flow CharacteristicsApplications: Suggested Uses Include Housewares, Storage Boxes, Containers, VialsInformation provided by Braskem
Physical Properties Metric English Comments
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength 35.2 MPa
5100 psi
2 in/min; ASTM D638
Elongation at Yield 10 %
10 %
2 in/min; ASTM D638
Flexural Modulus 1.34 GPa
195 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256A