SABIC Innovative Plastics LNP THERMOCOMP PFB55 PA 6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP PFB55 PA 6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* PFB55 is a compound based on PA 6 resin containing Glass Bead, Glass Fiber.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 155 MPa
22500 psi
5 mm/min; ISO 527
Elongation at Break 2.7 %
2.7 %
5 mm/min; ISO 527
Tensile Modulus 10.9 GPa
1580 ksi
1 mm/min; ISO 527
Flexural Yield Strength 229 MPa
33200 psi
2 mm/min; ISO 178
Flexural Modulus 10.0 GPa
1450 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 29.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
16.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
41.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
399 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af