Mechanical Properties Metric English Comments
Tensile Modulus 10.9 GPa
1580 ksi
Plastcom SLOVAMID 66 GF 25 FRA 5 PA66, 25% glass fibre, flame retardant
FeaturesPA 66 for injection moulding, reinforced with 25% glass fibre and halogen flame retardant. Application in electrical industry: breakers, coilforms, covers, terminals. Slightly decreased flam..
Tensile Modulus 10.9 GPa

@Temperature 23.0 °C
1580 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 74G33W NC010 Nylon 66  (Unverified Data**)
Zytel® 74G33W NC010 is a 33% glass reinforced nylon 66 and nylon 6 co-melt resin with improved weatherability.Information provided by DuPont Performance Polymers
Tensile Modulus 10.9 GPa
1580 ksi
ISO 527-1/-2
Kuraray Genestarâ„¢ GC1201A-M41 Nylon, Glass Filled and Carbon Filled
Reinforced injection grade for conductive applications.Main Features:ConductivityHeat resistanceChemical resistanceExample of applications:Quick connector
Tensile Modulus 10.9 GPa
1580 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral
Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature ran..
Tensile Modulus 10.9 GPa
1580 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP LF006EL PEEK (Europe-Africa-Middle East)
LNP* THERMOCOMP* LF006EL is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features include: Easy Molding. FDA Compliant Raw Materials.
Tensile Modulus 10.9 GPa
1580 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP PFB55 PA 6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* PFB55 is a compound based on PA 6 resin containing Glass Bead, Glass Fiber.
Tensile Modulus 10.9 GPa
1580 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP QF00A PA 6/10 (Europe-Africa-Middle East)
LNP* Thermocomp* QF00A is a compound based on Nylon 6/10 resin containing Glass Fiber.
Tensile Modulus 10.9 GPa
1580 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66 (Europe-Africa-Middle East)
LNP* Stat-kon* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Modulus 10.9 GPa
1580 ksi
ASTM D638
Plenco 3509 Phenolic, Granular, Transfer Molded
PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file..
Tensile Modulus 10.9 GPa
1580 ksi
ASTM D638
Plenco 4466 Phenolic, Granular, Compression Molded
PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466..
Tensile Modulus 10.9 GPa
1580 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 74G33W NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W NC010 is a 33% glass reinforced nylon 66 and nylon 6 co-melt resin with improved weatherability.Information provided by DuP..
Tensile Modulus 10.9 GPa
1580 ksi
Radici Radilon® A RV330 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Tensile Modulus 10.9 GPa
1580 ksi
After 7 days in boiling water
Gharda Chemicals GAFONE™ 3430GF PES, Glass Fiber-Reinforced  (discontinued **)
Glass fiber reinforced granules for injection molding. With lower viscosity for molding intricate cross sections.Characteristics: Very high rigidityGood dielectric propertiesHigh mechanical strengt..
Tensile Modulus 10.9 GPa
1580 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON PX06418 PA 6
LNP* VERTON* PX06418 is a compound based on Nylon 6 containing proprietary fillers. Added features of this grade are: Heat Stabilized, Structural.