Material Notes:
LNP* THERMOCOMP* MFB429 is a compound based on Polypropylene resin containing 10% Glass Fiber, 20% Glass Bead. Added features of this material include: Chemically Coupled, Flame Retardant.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 41.0 MPa
5950 psi
ASTM D638
Elongation at Break 2.6 %
2.6 %
ASTM D638
Tensile Modulus 5.58 GPa
809 ksi
50 mm/min; ASTM D638
Flexural Strength 68.0 MPa
9860 psi
ASTM D790
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
Izod Impact, Notched 0.420 J/cm
0.787 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.67 J/cm
5.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 130 °C

@Thickness 3.20 mm
266 °F

@Thickness 0.126 in
unannealed; ASTM D648