Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Resistalloy International Resistalloy 6015 Nickel Chromium Electrical Resistance Alloy

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Resistalloy International Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resistalloy International Resistalloy 6015 Nickel Chromium Electrical Resistance Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of atmospheres. Available as wire and strip. Slightly magnetic.Information provided by Resistalloy International Limited.
Physical Properties Metric English Comments
Density 8.20 g/cc
0.296 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 180
180
Tensile Strength, Ultimate 750 MPa
109000 psi
100 MPa

@Temperature 900 °C
14500 psi

@Temperature 1650 °F
Tensile Strength, Yield 450 MPa
65300 psi
Elongation at Break 25 - 30 %

@Thickness 50.0 mm
25 - 30 %

@Thickness 1.97 in
Thermal Properties Metric English Comments
CTE, linear 14.0 µm/m-°C

@Temperature 20.0 - 250 °C
7.78 µin/in-°F

@Temperature 68.0 - 482 °F
15.0 µm/m-°C

@Temperature 20.0 - 500 °C
8.33 µin/in-°F

@Temperature 68.0 - 932 °F
17.0 µm/m-°C

@Temperature 20.0 - 1000 °C
9.44 µin/in-°F

@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.460 J/g-°C
0.110 BTU/lb-°F
Thermal Conductivity 13.0 W/m-K
90.2 BTU-in/hr-ft²-°F
Melting Point 1390 °C
2530 °F
Maximum Service Temperature, Air 1150 °C
2100 °F
Optical Properties Metric English Comments
Emissivity (0-1) 0.88
0.88
Fully Oxidized
Component Elements Properties Metric English Comments
Chromium, Cr 15 %
15 %
Iron, Fe 25 %
25 %
Nickel, Ni 60 %
60 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000111 ohm-cm
0.000111 ohm-cm
Temperature Factor is 1.10 at 800°C (1470°F). Temperature Factor is 1.11 at 1000°C (1830°F). Temperature Factor is 1.13 at 1200°C (2190°F).
Users viewing this material also viewed the following: