Polymer Property : Melting Point = 2530 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1390 - 1440 °C
2530 - 2620 °F
Kennametal Stellite Denertiaâ„¢ C4 Cobalt Chromium Dental Alloy
Denertia™ C4 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework.It conforms to the following International Standards: EN 1641 §4...
Melting Point 1390 - 1430 °C
2530 - 2610 °F
Special Metals INCONEL® Alloy 751
A nickel-chromium alloy similar to INCONEL ALLOY X-750 but with increased aluminum content for greater precipitation hardening. INCONEL alloy 751 was designed for use as exhaust valves in internal-..
Melting Point 1390 - 1430 °C
2530 - 2610 °F
Special Metals INCONEL® Alloy X-750
A nickel-chromium alloy similar to INCONEL alloy 600 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good resistance to corrosion and oxidation along with hig..
Melting Point 1390 °C
2530 °F
Goodfellow Zirconium 56.5/Vanadium 43.5 Alloy
Information provided by Goodfellow.
Melting Point 1388 °C
2530 °F
ATI Allegheny Ludlum AL 22™ Nickel-Base Alloy, UNS N06022
AL 22 alloy is a Ni-Cr-Mo alloy that provides outstanding resistance to pitting, crevice corrosion, intergranular attack, and stress corrosion cracking. The combination of Cr, Ni, Mo, and W provide..
Melting Point 1390 - 1440 °C
2530 - 2620 °F
ATI Allegheny Ludlum Type 317 Stainless Steel, UNS S31700
This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels ..
Melting Point 1390 - 1440 °C
2530 - 2620 °F
ATI Allegheny Ludlum Type 316 Stainless Steel, UNS S31600
This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels ..
Melting Point 1390 - 1440 °C
2530 - 2620 °F
ATI Allegheny Ludlum Type 316L Stainless Steel, UNS S31603
This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels ..
Melting Point 1390 °C
2530 °F
Resistalloy International Resistalloy 3718 Nickel Chromium Electrical Resistance Alloy
Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at..
Melting Point 1390 °C
2530 °F
Resistalloy International Resistalloy 6015 Nickel Chromium Electrical Resistance Alloy
Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at..