Features:Medium FlowHigh Thermal ResistantMechanical StrengthFDA Rating: 21 CFR 177.1640Applications:Extrusion/ThermoformingInjectionDisposablesGPPS/HIPS BlendsInformation provided by US distributor Calsak Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
ASTM D955
Melt Flow 3.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.2 MPa
3650 psi
ASTM D638
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Break 61 %
61 %
ASTM D638
Tensile Modulus 2.068 GPa
299.9 ksi
ASTM D638
Izod Impact, Notched 0.720 J/cm
1.35 ft-lb/in
0.5 in.; ASTM D256
0.910 J/cm
1.70 ft-lb/in
0.125 in.; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Flammability, UL94 HB
HB