Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Multibase Multi-Pro® 4015 THW Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L8230 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M4825 Polyvinyl Chloride, Rigid (PVC, Rigid) ** NOTE: UL REGULATORY LISTING PENDINGInformation provided by PolyOne |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Oxford Polymers PC 10GF-V0 UL Listed Polycarbonate UL Listed PolycarbonateInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Ineos Nova 1210 High Heat Crystal Polystyrene
(discontinued **) High heat resistance, High molecular weight, optimum performance in extruded foamApplications: Meat and poultry trays, Egg cartons, Food packagingExposure to gamma radiation in the 2.02-6.06 megarad.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Ineos Nova 1230 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Flexural Modulus | 3.24 - 10.9 GPa | 470 - 1580 ksi | Average value: 7.78 GPa Grade Count:62 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Polymer Resources PEI-GP1 Polyetherimide, General Purpose, Unreinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM Data |
BASF Capron® 5202 HS BK-102 Nylon 66 (Dry)
(discontinued **) Capron 5202 HS BK-102 is an unfilled, heat stabilized, pigmented black nylon 6,6, injection molding compound. It combines strength and stiffness as well as excellent chemical resistance. The additi.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
LG Chemical LUPOL GP-3154F General Purpose Polypropylene, 15% Mineral Fillers, High Modulus, Flame Retardant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 9076 PEI Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem LTX300A PEI Copolymer (Europe-Africa-Middle East) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF10 IM L BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Com.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF6 L BK 6% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 6% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF7 L 7% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 7% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Techmer ES HiFill® POM HO UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: HomopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer (Asia Pacific) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Chase Plastics CP Pryme® PC310R Polycarbonate, 10% Glass Fiber Reinforced, Recycled Content Features: Good mold releaseRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Videolar 585 Crystal Polystyrene (GPPS) High heat extrusion crystalSuperior oriented polystyrene sheetFeatures: Low melt flowHigh molecular weightApplications: Foam applications such as egg cartons, meat trays and food serviceSuperior ori.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Asahi Kasei Thermylene® P-20FG-1740 20% Glass Fiber Reinforced, Medium Impact Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Americas Styrenics EA3130 High Heat Crystal Polystyrene Product CharacteristicsAdditive FreeFood Contact CompliantTypical ApplicationsMedical PartsColor Concentrate CarrierLow Profile AdditivesInformation provided by AmericasStyrenics LLC. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Americas Styrenics STYRON® 685D High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceHigh tensile strengthBlue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsFoamOPSMedicalInformation provided by AmericasSty.. |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-20FG-0754 20% Glass, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.24 GPa | 470 ksi | ASTM D790 |
Americas Styrenics STYRON® 695 High Heat Crystal Polystyrene Product CharacteristicsReduced residualsHigh heat resistancehigh strengthFood Contact CompliantTypical ApplicationsOPSInformation provided by AmericasStyrenics LLC. |