Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering V70Q Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering V70Q Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Black, Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. ASTM designation = FKM. ISO designation = FPM. Formulated using only those ingredients determined by the United States Food and Drug Administration (FDA) in accordance with Code of Federal Regulations Title 21 (CFR21) Part 177.2600.Applications: FDA grade, formulated for use as product contact surfaces in dairy equipment.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
°IRHD; ASTM D1415
60 - 80
60 - 80
°IRHD, ±10 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 9.00 MPa
1310 psi
-25% change after 72 hours @ 250°C; ASTM D412
12.0 MPa
1740 psi
ASTM D412
Elongation at Break 150 %
150 %
-25% change after 72 hours @ 250°C; ASTM D412
200 %
200 %
ASTM D412
Compression Set 35 %
35 %
22 hours @ 175°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Flash Point >= 315 °C
>= 599 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved