Polyram PlusTek PA108 Nylon6/6.6 Alloy for Injection Molding

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, Unreinforced
Manufacturer Polyram
Trade Name PlusTek
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PA108 Nylon6/6.6 Alloy for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good surface finish Nylon 6/6.6 alloy for injection molding.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 2.8 %
2.8 %
50% RH; ISO 62
Water Absorption at Saturation 8.5 %
8.5 %
ISO 62
Linear Mold Shrinkage 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
ISO 2577
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
Tensile Strength, Yield 90.0 MPa
13100 psi
ISO 527
Elongation at Break 25 %
25 %
ISO 527
Flexural Strength 140 MPa
20300 psi
ISO 178
Flexural Modulus 3.00 GPa
435 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
ISO 11357
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous use
200 °C
392 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75
Flammability, UL94 V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
Glow Wire Test 750 °C
1380 °F
GWFI; IEC 60695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.6

@Frequency 1.00e+6 Hz
3.6

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 120 kV/mm
3050 kV/in
IEC 60250