Polyphosphazene Rubber (PZ, FZ)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyphosphazene Rubber (PZ, FZ).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FZ refers to the fluorinated (55 wt%) polymer.
Physical Properties Metric English Comments
Density 1.75 - 1.90 g/cc
0.0632 - 0.0686 lb/in³
Compounded
Mechanical Properties Metric English Comments
Hardness, Shore A 35 - 90
35 - 90
Depends on compounding
Tensile Strength, Ultimate 14.0 MPa
2030 psi
Compounded Tire
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 175 °C
347 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F