Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB POLYform POM C M90 S10 Polyoxymethylene, Impact Modified

Category Polymer , Thermoplastic
Manufacturer Polykemi AB
Trade Name POLYform
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYform POM C M90 S10 Polyoxymethylene, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Linear Mold Shrinkage 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
With Flow; ISO 2577
0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
Across Flow; ISO 2577
Melt Index of Compound 9.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 45.0 MPa
<= 6530 psi
ISO/R527
Elongation at Yield 7.0 %
7.0 %
ISO/R527
Flexural Strength <= 80.0 MPa
<= 11600 psi
ISO 178
Flexural Modulus 2.00 GPa

@Temperature 23.0 °C
290 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
120°C/h; ISO 75/1
Vicat Softening Point 140 °C

@Load 5.001 kg
284 °F

@Load 11.03 lb
50°C/h; ISO 306
Copyright © lookpolymers.com All Rights Reserved