Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Trilliant™ HC HC5220-0040 RS Natural Polypropylene, Unspecified (PP, Unspecified)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer PolyOne Corporation
Trade Name Trilliant™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Trilliant™ HC HC5220-0040 RS Natural Polypropylene, Unspecified (PP, Unspecified).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead of the competition. When specified, Trilliant® compounds may incorporate agency rated materials that meet USP Class VI, FDA or ISO 10993 testing requirements.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 57.9 MPa
8400 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 1.0 %
1.0 %
Type I, 51 mm/min; ASTM D638
Flexural Strength 88.9 MPa
12900 psi
ASTM D790
Flexural Modulus 6.79 GPa
985 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.806 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Izod Impact, Unnotched 2.10 J/cm
3.93 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 204 - 216 °C
399 - 421 °F
Deflection Temperature at 0.46 MPa (66 psi) >= 155 °C

@Thickness 3.18 mm
>= 311 °F

@Thickness 0.125 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
Annealed; ASTM D648
Processing Properties Metric English Comments
Mold Temperature 26.7 - 37.8 °C
80.1 - 100 °F
Descriptive Properties Value Comments
Agency Ratings USP Class VI
Appearance Natural Color
Features Biocompatible
Good Chemical Resistance
Good Colorability
Specialty Grade
Filler / Reinforcement Glass Fiber Reinforcement, 40% Filler by Weight
Forms Pellets
Generic Material PP, Unspecified
Generic Name Polypropylene, Unspecified (PP, Unspecified)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Hospital Goods
Medical/Healthcare Applications