Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.79 GPa | 985 ksi | ASTM D790 |
PolyOne Trilliant™ HC HC5220-0040 RS Natural Polypropylene, Unspecified (PP, Unspecified) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Flexural Modulus | 6.79 GPa | 985 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ZFL34 PPE+PS LNP* LUBRICOMP* ZFL34 is a compound based on PPE+PS resin containing 20% Glass Fiber, 15% PTFE. Added feature of this gradae is: Wear Resistant. |
|||
Flexural Modulus | 6.79 GPa | 985 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp ZFL34 PPO LNP* Lubricomp* ZFL34 is a compound based on Modified PPO containing glass fiber and PTFE.This data was supplied by SABIC-IP for the Americas region. |