Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Synprene® ST-6240 Thermoplastic Elastomer - SBC  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® ST-6240 Thermoplastic Elastomer - SBC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Over-Molding GradeUV StabilizedApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
5 sec; ASTM D2240
Tensile Strength, Yield 7.65 MPa
1110 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
1.86 MPa

@Strain 100 %
270 psi

@Strain 100 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
3.72 MPa

@Strain 300 %
540 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 740 %
740 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 29.8 kN/m
170 pli
Die C (graves), 20 in/min; ASTM D624
Copyright © lookpolymers.com All Rights Reserved