PolyOne Synprene® RT-3830MS Thermoplastic Elastomer - SBC  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® RT-3830MS Thermoplastic Elastomer - SBC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTransparentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
0.900 g/cc
0.900 g/cc
ASTM D792
Linear Mold Shrinkage 0.019 cm/cm
0.019 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Instant; ASTM D2240
30
30
Instant; ASTM D2240
Tensile Strength, Yield 4.41 MPa
640 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
4.41 MPa
640 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
1.59 MPa

@Strain 300 %
230 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
1.59 MPa

@Strain 300 %
230 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 725 %
725 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
725 %
725 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Rebound 60 %
60 %
Bayshore; ASTM D2632
Tear Strength 16.7 kN/m
95.0 pli
Die C (graves), 20 in/min; ASTM D624
16.7 kN/m
95.0 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 20 %
20 %
Method B, 73°F(23°C), 22 hrs; ASTM D395
20 %
20 %
Method B, 73°F(23°C), 22 hrs; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -65.0 °C
-85.0 °F
ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified