Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | Across Flow; ISO 294-4 |
PolyOne Versalloy™ HC 9220-70 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-70 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | Across Flow; ISO 294-4 |
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ASTM D955 |
Noble Polymers Forte™ 4CPP093 Nanocomposite Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | 0.125 in; ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (DAM) Information provided by Ravago |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | STN 64 0808 |
Plastcom SLOVALEN PQ 91 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Linear Mold Shrinkage | 0.019 - 0.022 cm/cm | 0.019 - 0.022 in/in | after bake; ISO 294 |
Solvay Engineered Polymers DEXFLEX® 810HSF TPO
(discontinued **) Description: DEXFLEX® 810HSF is a thermoplastic olefinic elastomer (TPO) designed for large molded-in-color automotive exterior applications that require high flow characteristics for excellent pro.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | 0.125 in, DAM; ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (Cond) Information provided by Ravago |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | 0.125 in, DAM; ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000STL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | 0.125 in; ASTM D955 |
Ravago Manufacturing Americas Hylon® N1000STL Nylon 6/6 (DAM)
(discontinued **) Information provided by Entec. |
|||
Linear Mold Shrinkage | 0.019 - 0.030 cm/cm | 0.019 - 0.030 in/in | |
Lehmann & Voss LUVOCOM® 80-8444 Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.dynamic stressReduced moment of inertia compared with metal parts.Isotropic shrinkage character.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ASTM D955 |
Kolon KOCETAL® CB301 Conductive Grade Acetal Resin Conductive grade. Applications: Conductive products. Information provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ISO 294-4 |
Aardvark Polymers AARTEL® 800 Rotational Molding Resin Aartel 800 is our high test, general purpose, acetal copolymer. Aartel 800 provides overall excellent performance for most applications and is available in natural (off white) and a wide range of st.. |
|||
Linear Mold Shrinkage | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ASTM D955 |
Kolon KOPA® KN333HFBL General Purpose Nylon 66 Middle viscosity, flexibleApplications Band cables for vehiclesInformation provided by API-Kolon. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ISO 294-4 |
Gromax 1172LL TPE 1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ASTM D955 |
Multibase Multi-Flex® A 7202 MR TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | RHODIA-EP |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Linear Mold Shrinkage | 0.019 - 0.025 cm/cm | 0.019 - 0.025 in/in | ASTM D955 |
Teknor Apex Chemlon® 109 Nylon 66, Impact Grade Notes: High-Impact; Exceptional impact strength, especially at low temperatures; FMVSS Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | RHODIA-EP |
Solvay Technyl® A 205F Nylon 66, EH0 Unreinforced polyamide 66, high fluidity, fast cycling grade, for injection molding.Technyl A 205F offers two main advantages: excellent filling qualities and UL 94 V2 under 0.4 mm. It is particula.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ASTM D955 |
Tipco Tipcolene® PPH-OIT - Unfilled Polypropylene Homopolymer Compound with Copper Inhibitor (Metal Deactivator) PP Homopolymer with Copper Inhibitor (Metal De-activator)Applications: Automotives & ElectricalProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | |
Polyram RamTal PM340S4 Acetal, 20% Glass beads Reinforced 20% Glass beads reinforced polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.019 - 0.025 cm/cm | 0.019 - 0.025 in/in | |
Polyram RamTal PM1419 Acetal, PTFE Filled Polyacetal filled with PTFE for sliding parts, low friction and improved wear resistance in molded parts.Information provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ASTM Data; MD |
BASF Ultraform N 2640 Z4 UNC Q600 POM Ultraform N2640 Z4 UNC Q600 is a high toughness, elastomer-modified injection molding POM grade. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ASTM Data; MD |
BASF Ultraform N 2640 Z6 UNC POM Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | |
Advanced Polymer Alloys DuraGrip™ 6150 BK Melt Processable Elastomer DuraGrip™ 6150BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6150BK has an excellent
soft touch feel a.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ASTM D955 |
Ascend Performance Materials VYDYNE® 45 Nylon, Impact Modified, Weather Stable Typical property data. VYDYNE is a registered trademark of Solutia Inc. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | |
Plastcom SLOVALEN PH 91 GF 10 PP, 10% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fibre. Increased strength in comparison with unfilled PP. Applied in all industry branches. Increased str.. |
|||
Linear Mold Shrinkage | 0.019 cm/cm | 0.019 in/in | ASTM D955 |
PolyOne Synprene® RT-3830MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTransparentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |